Seite - 1680 - in Book of Full Papers - Symposium Hydro Engineering
Bild der Seite - 1680 -
Text der Seite - 1680 -
1. SUMMARY OF P.LH CEMENT DEVELOPMENT
C2S is main component in P.LH cement, which was used in Hoover dam in
30’s last century. After Hoover dam completed, concrete strength has increased
slowly[4][5]. C2S content in Hoover dam is 46%[4] and US national standards ASTM
C150 specified the C2S content should be over 40%[7]. As lower early strength,
difficult production and high cost, P.LH cement was no longer produced and applied
in US after 50’s and ASTM IV was only remained in US standard list[8].
C2S is functioned as lower hydration heat, less water consumption, high step-
up strength in late age and well durability, which has incomparable superiority in
comparison with C3S. There are two difficulties existed in traditional calcing
process while high C2S content cement produced, one is how to remain stability of
β-C2S crystal type to prevent transformation to γ-C2S basically without hydration
activation, the other is how to excite C2S hydration activation to avoid lower early
strength in normal ambient temperature, for instance, 7d strength is only 7MPa in
accordance with US standard ASTM IV. Breakthrough of high C2S cement research
and production in China were made to realize industrial production and large-scale
application with C2S≥40% as dominant mineral. Chinese standard Moderate Heat
Portland Cement, Low Heat Portland Cement and Low Heat Portland Slag Cement
[9](GB 200-2003) was published to specify 7d strength of P.LH cement shall be not
less than 13MPa.
In the early study and research, consideration has only been taken how to
realize higher C2S content in P.LH. With high C3A but lower MgO content, P.LH
cement was milled finer such that the complicated crack resistance performance
would not get obviously different while compared with concrete mixed with P.MH
cement[16][17]. It is necessary to optimize P.LH research on the current basis to meet
the requirement of ultra arch dam .
2. P.LH CEMENT CHARACTERISTICS APPLIED FOR ULTRA ARCH DAM
The match of clinker’s mineral composition, physical performance and overall
performance of P.LH cement applied shall be optimized in ultra-high dam .
While C2S is over 40%, C3S will be increased properly to ensure that total
quantity of silicate mineral is greater than 75% to guarantee a certain early strength.
Simultaneously a certain flux mineral(C3A and C4AF) shall be existed. In
consideration of durability, properly increase C4AF and decrease C3A in P.LH
cement. Therefore the law of cement strength and hydration influenced by silicate
1680
Book of Full Papers
Symposium Hydro Engineering
- Titel
- Book of Full Papers
- Untertitel
- Symposium Hydro Engineering
- Autor
- Gerald Zenz
- Verlag
- Verlag der Technischen Universität Graz
- Ort
- Graz
- Datum
- 2018
- Sprache
- englisch
- Lizenz
- CC BY-NC-ND 4.0
- ISBN
- 978-3-85125-620-8
- Abmessungen
- 20.9 x 29.6 cm
- Seiten
- 2724
- Schlagwörter
- Hydro, Engineering, Climate Changes
- Kategorien
- International
- Naturwissenschaften Physik
- Technik